Search published articles


Showing 2 results for Ranjbar Motlagh

Sasan Ranjbar Motlagh, Hosein Momeni, Naser Ehsani,
Volume 18, Issue 1 (March 2021)
Abstract

In this study, the effect of annealing treatment on microstructure and mechanical properties of Nb-10Hf-1Ti wt.% produced by Spark Plasma Sintering (SPS) was investigated. Scanning electron microscope (SEM), optical microscopy, X-ray diffraction analysis, hardness, and uniaxial tension test were used. Annealing treatment was carried out in a vacuum of 10-3 Pa at 1150 °C for 1, 3, 5, and 7 hours and in an argon atmosphere at 1350 °C for 5 hours. Internal oxidation and subsequent hafnium oxide formation causes the hardening of the C103 alloy and drastically increases hardness and tensile strength. Although HfO2 particles formed in the grain boundary cause brittleness and cleavage fracture of samples. Volume fraction, particle size, and mean interparticle spacing of oxides significantly change by annealing and subsequently the mechanical properties are affected. The SPSed sample at 1500 ℃ is softened by annealing at 1150 ℃ for 5 hours and its hardness and yield strength are reduced from 303 Hv to 230 Hv and 538 MPa to 490 MPa respectively. While annealing at 1350 ℃for 5 hours increases hardness and yield strength increases to 343 Hv and 581 MPa. 
Hossein Momeni, Sasan Ranjbar Motlagh,
Volume 21, Issue 3 (September 2024)
Abstract

The present work deals with the hot deformation behavior of commercial Nb alloy C-103 and its microstructure evolution during uniaxial compression tests in the temperature range of 700-1100 °C and the strain rate range of 0.001-0.4 s-1. Strain rate sensitivity, calculated from the compression tests data, was almost constant and showed a negative value in the temperature range of 700-900 °C but increased significantly beyond 900 °C. Dynamic strain aging was found to have a predominant effect up to 900 °C, beyond which dynamic recovery and oxidation influenced the compressive properties. The microstructure of the deformed samples showed indications of dynamic recrystallization within the high strain rate sensitivity domain and features of flow instability in the regime of low strain rate sensitivity. The 950–1000 °C temperature range and strain rate range of 0.001-0.1 s-1 were suggested as suitable hot deformation conditions. The constitutive equation was established to describe the alloy's flow behavior, and the average activation energy for plastic flow was calculated to be 267 kJ/mol.
 

Page 1 from 1     

© 2022 All Rights Reserved | Iranian Journal of Materials Science and Engineering

Designed & Developed by : Yektaweb